logo
Wuhan Fengfan International Trade Co.,Ltd. 86-27-85615818 info@fengfan.net
High Temperature Zn-618 Brightener for Acidic Zinc Plating with High Gloss and Good Leveling Ability

High Temperature Zn-618 Brightener for Acidic Zinc Plating with High Gloss and Good Leveling Ability

  • Evidenziare

    High Temperature Zn-618 Brightener

    ,

    High Gloss Acidic Zinc Plating Brightener

    ,

    Good Leveling Ability Zinc Plating Additive

  • Utilizzo
    Zinco
  • Imballaggio
    25 kg per secchio
  • Caratteristica
    alta lucidatura e capacità di livellamento
  • Luogo di origine
    Cina
  • Marca
    FENGFAN
  • Numero di modello
    Zn-618
  • Quantità di ordine minimo
    Negoziabile
  • Prezzo
    Negoziabile
  • Imballaggi particolari
    Packaging di esportazione standard
  • Tempi di consegna
    15-25 giorni di lavoro
  • Termini di pagamento
    L/C, D/A, D/P, T/T, Western Union, MoneyGram
  • Capacità di alimentazione
    200000pcs/giorno

High Temperature Zn-618 Brightener for Acidic Zinc Plating with High Gloss and Good Leveling Ability

High temperature Zn-618 Brightener for Acidic Zinc Plating


1. Properties

1. It is composed by primary brightener and auxiliary one, it owns high gloss and leveling ability.

 

2. High current efficiency, good leveling ability, as well as stable.

 

3. Good heat resistance, suitable for no refrigeration equipment manufacturers.

 

4. Both rack and barrel plating additive suitable for processing of complex parts.

 

                       

2. Bath composition and Operation condition

Bath composition and Operation condition:

Rack plating   

Barrel plating

ZnCl2

60~70g/L

45~60g/L

KCl

180~220g/L

200~240g/L

H3BO3

25~35g/L

25~35g/L

ZN-618A

0.3~1ml/L

0.3~1ml/L

ZN-618B

30~40ml/L

30~40ml/L

Cathnode current density(Dk)

0.5~5A/dm2

0.1~3A/dm2

PH

4.5~6.0

4.5~6.0

SK:SA

1:1.5~2

1:1.5~2

Anode

0zinc ingot

0zinc ingot

 

3. Solution Make-up

Add water at the 2/3 amount of bath volume, then add above amount of KCl and ZnCl2 and stir. Dissolve H3BO3 with 80℃ hot water and add slowly into the bath, then add 1-2g/L zinc powder, stir 20-30 minutes, Filter into the bath after solution becomes clarified, add water according to calculated volume. Dissolve above calculated Zn-618 additive by one time of volume water and add into the bath, stir uniform, then start to do trial plating.